Common Issues with PVC Conduit and Industrial-Grade Solutions

🌲🔖📌Rough pipe surface with pitting

💫Uneven raw material mixing, insufficient lubricant; low extrusion temperature, poor melt plasticization 🌳1. Adjust formulation; 2. Optimize mixing process; 3. Adjust extrusion temperature

🌲🔖📌Bubbles or pinholes on pipe inner wall

💫📍Moisture in raw material (PVC resin absorbs moisture), excessive volatiles in formulation; Insufficient vacuum in sizing tank

🌳 1. Pre-treat raw material; 2. Optimize formulation; 3. Adjust equipment settings

🌲🔖📌Uneven wall thickness, excessive ovality

💫Mold core misalignment, unstable haul-off speed; sizing sleeve misaligned with mold center 🌳1. Calibrate equipment; 2. Stabilize haul-off; 3. Correct sizing sleeve alignment

🌲🔖📌Pipe prone to breakage, poor impact resistance

💫Insufficient toughening agent, excessive calcium carbonate; rapid cooling causing internal stress concentration

🌳1. Adjust formulation; 2. Optimize cooling process; 3. Select high-impact PVC resin

🌲🔖📌Pipe compressive strength fails to meet standard (≤1.0MPa)

💫Low raw material purity, improper reinforcing filler ratio; Insufficient extrusion pressure, low melt density

🌳1. Upgrade raw materials; 2. Adjust formulation; 3. Adjust equipment settings

🌲🔖📌Pipe cut edges crack or exhibit burrs

💫Excessive cutting speed, dull blades; pipes not fully cooled and set

🌳1. Perform equipment maintenance; 2. Extend cooling time; 3. Treat cut edges

🌲🔖📌Pipes age and become brittle during use (outdoor applications)

💫Absence of antioxidants and UV absorbers; thermal stabilizers in formulation degraded

🌳1. Optimize formulation; 2. Use weather-resistant additives; 3. Surface treatment: Apply film coating or anti-aging coating to outdoor pipes